Please use this identifier to cite or link to this item: https://ir.swu.ac.th/jspui/handle/123456789/17420
Full metadata record
DC FieldValueLanguage
dc.contributor.authorKraipok A.
dc.contributor.authorIntawin P.
dc.contributor.authorKamnoy M.
dc.contributor.authorInthong S.
dc.contributor.authorLeenakul W.
dc.contributor.authorBintachitt P.
dc.contributor.authorEitssayeam S.
dc.contributor.authorKhamman O.
dc.contributor.authorTunkasiri T.
dc.contributor.authorPengpat K.
dc.date.accessioned2022-03-10T13:17:02Z-
dc.date.available2022-03-10T13:17:02Z-
dc.date.issued2021
dc.identifier.issn18206131
dc.identifier.other2-s2.0-85117929505
dc.identifier.urihttps://ir.swu.ac.th/jspui/handle/123456789/17420-
dc.identifier.urihttps://www.scopus.com/inward/record.uri?eid=2-s2.0-85117929505&doi=10.2298%2fPAC2103238K&partnerID=40&md5=a547f21d3893a8adfdeeb0f2f136b743
dc.description.abstractLithium disilicate (LD) glass-ceramics are extensively employed in restorative dentistry because their superior aesthetic properties and hardness are similar to natural teeth. The aim of this work is to investigate the mechanical properties and chemical solubility of lithium disilicate glass-ceramics prepared by the low-pressure injection moulding using the PEG-based binder. The glass-to-binder ratio was varied as 60:40, 55:45, 50:50 and 45:55 vol.%. The sintering conditions of 800 °C with 2 h dwell time were selected according to thermal analysis. Phase formation, microstructure and mechanical properties of the prepared samples were characterized by XRD, SEM, microhardness and three-point bending test, respectively. Besides, the chemical solubility of the system was investigated by the immersion test in acetic acid solution. XRD analyses of the sintered sample confirmed the presence of only one prominent crystalline phase of LD. SEM result showed that the porosity increased with decreasing glass powder content. The mechanical properties of the LD glass-ceramic samples tended to decrease when the proportion of the glass powder decreased, while the chemical solubility tended to increase. The mechanical properties of the glass-ceramics, i.e. the highest density value, Vickers hardness and flexural strength were 2.55 g/cm3, 6.80 GPa, and 176 MPa, respectively. These results could be useful in developing these LD glass-ceramics for their optimal use in dental applications. © 2021 University of Novi Sad, Faculty of Technology. All rights reserved.
dc.languageen
dc.titleEffect of PEG-based binder concentration on the mechanical properties of lithium disilicate glass-ceramics prepared by low-pressure injection moulding
dc.typeArticle
dc.rights.holderScopus
dc.identifier.bibliograpycitationProcessing and Application of Ceramics. Vol 15, No.3 (2021), p.238-245
dc.identifier.doi10.2298/PAC2103238K
Appears in Collections:Scopus 1983-2021

Files in This Item:
There are no files associated with this item.


Items in SWU repository are protected by copyright, with all rights reserved, unless otherwise indicated.