dc.contributor.author | Kraipok A. | |
dc.contributor.author | Intawin P. | |
dc.contributor.author | Bintachitt P. | |
dc.contributor.author | Leenakul W. | |
dc.contributor.author | Khamman O. | |
dc.contributor.author | Eitssayeam S. | |
dc.contributor.author | Tunkasiri T. | |
dc.contributor.author | Pengpat K. | |
dc.date.accessioned | 2022-03-10T13:17:01Z | - |
dc.date.available | 2022-03-10T13:17:01Z | - |
dc.date.issued | 2021 | |
dc.identifier.issn | 1546542X | |
dc.identifier.other | 2-s2.0-85118567642 | |
dc.identifier.uri | https://ir.swu.ac.th/jspui/handle/123456789/17412 | - |
dc.identifier.uri | https://www.scopus.com/inward/record.uri?eid=2-s2.0-85118567642&doi=10.1111%2fijac.13945&partnerID=40&md5=43a2a16c835db08b466dad1d3b3d5961 | |
dc.description.abstract | This study aims to investigate the influence of heat treatment temperatures on the mechanical properties and chemical solubility (CS) of lithium disilicate-fluorcanasite glass-ceramics and to develop new dental materials. The glasses and glass-ceramics were prepared using CaF2-SiO2-CaO-K2O-Na2O-Li2O-Al2O3-P2O5-based glass system using a conventional melt quenching method followed by a two-stage crystallization process. This two-stage method involves two heating temperature steps: first at a constant temperature (TS1) of 600°C and second step at varying temperatures (TS2) of 650, 700, 750, and 800°C. The crystallization behavior, phase formation, microstructure, translucency characteristic, density, hardness, fracture strength, and CS were investigated. It was found that the lithium disilicate crystal acted as the main crystalline phase, and the crystalline phase of fluorcanasite occurred at the heat treatment temperatures of 750 and 800°C. In addition, it was found that density, hardness, fracture strength, and CS increased while the translucency values decreased with increasing heat treatment temperatures. Furthermore, the CS increased dramatically when the fluorcanasite phases occurred in the glass-ceramic samples. The maximum density values, Vickers hardness, fracture toughness, and flexural strength are 2.56 g/cm3, 6.73 GPa, 3.38 MPa.m1/2, and 259 MPa, respectively. These results may offer a possibility to design a new material for dental applications based on lithium disilicate-fluorcanasite glass-ceramics. © 2021 The American Ceramic Society | |
dc.language | en | |
dc.subject | Alumina | |
dc.subject | Aluminum oxide | |
dc.subject | Calcium fluoride | |
dc.subject | Crystallization | |
dc.subject | Dental materials | |
dc.subject | Durability | |
dc.subject | Fluorspar | |
dc.subject | Fracture toughness | |
dc.subject | Heat treatment | |
dc.subject | Lithium compounds | |
dc.subject | Silica | |
dc.subject | Sodium compounds | |
dc.subject | Vickers hardness | |
dc.subject | Chemical durability | |
dc.subject | Chemical solubility | |
dc.subject | Crystalline phasis | |
dc.subject | Dental replacement | |
dc.subject | Fluorcanasite | |
dc.subject | Glass-ceramics | |
dc.subject | Heat treatment temperature | |
dc.subject | Lithium disilicate | |
dc.subject | Lithium disilicate-fluorcanasite | |
dc.subject | Property | |
dc.subject | Glass ceramics | |
dc.title | Influence of heat treatment temperature on the properties of the lithium disilicate-fluorcanasite glass-ceramics | |
dc.type | Article | |
dc.rights.holder | Scopus | |
dc.identifier.bibliograpycitation | International Journal of Applied Ceramic Technology. Vol , No. (2021) | |
dc.identifier.doi | 10.1111/ijac.13945 | |
Appears in Collections: | Scopus 1983-2021 |
Files in This Item:
There are no files associated with this item.
Items in SWU repository are protected by copyright, with all rights reserved, unless otherwise indicated.