Keywords: | Columns (structural) Deformation Energy dissipation Failure (mechanical) Glass fibers Shear strength Strain American Concrete Institute Deformation capacity Energy dissipation capacities Experimental program Flexural reinforcement Glass fiber reinforced polymer Longitudinal strain Shear strengthening Fiber reinforced plastics |
Issue Date: | 2021 |
Abstract: | The results of an experimental program on shear-strengthening of flat slabs using Glass Fiber Reinforced Polymer (GFRP) rods are presented. A total of seven specimens were tested under an upward concentric monotonic loading until failure. One specimen served as a control and was tested without any modification. The remaining six specimens were strengthened with post-in-stalled GFRP rods in single (SG), double (DB), and radial (RD) patterns within shear critical parameters around the centric column. The results of this experimental study suggest that GFRP rods are capable of enhancing both the peak load and deformation capacity. Furthermore, brittle failure associated with punching shear failure was successfully avoided by all strengthening patterns. Of all of the patterns, the RD pattern resulted in maximum peak load increase and corresponding deformation capacity while the lowest bound was created by the SG pattern. The results suggested that SG, DB and RD patterns enhanced ultimate loads up to 9.1, 11.3 and 15.7% while corresponding deflections increased up to 109, 136 and 154%. Strain measurement on flexural reinforcement suggested that all strengthened specimens were able to withstand higher longitudinal strains than yield. It was further shown that reducing the spacing between the GFRP rods efficiently enhanced peak loads, nevertheless, neither this change was proportional, nor did it result in an enhanced energy dissipation capacity. In the end, recommendations of American Concrete Institute (ACI) for the shear strength of two-way systems were modified to incorporate the contributions from GFRP rods. The results indicate that the proposed analytical approach provides an excellent match with the experimental results. © 2021 by the authors. Licensee MDPI, Basel, Switzerland. |
URI: | https://ir.swu.ac.th/jspui/handle/123456789/17234 https://www.scopus.com/inward/record.uri?eid=2-s2.0-85111579934&doi=10.3390%2fpolym13142369&partnerID=40&md5=7a3822f63a6a3f07f57e65e789dda238 |
ISSN: | 20734360 |
Appears in Collections: | Scopus 1983-2021 |
Files in This Item:
There are no files associated with this item.
Items in SWU repository are protected by copyright, with all rights reserved, unless otherwise indicated.