Please use this identifier to cite or link to this item:
https://ir.swu.ac.th/jspui/handle/123456789/13174
Full metadata record
DC Field | Value | Language |
---|---|---|
dc.contributor.author | Wongpreedee K. | |
dc.contributor.author | Peerawat A. | |
dc.contributor.author | Phichaikamjornwut B. | |
dc.contributor.author | Bootkul D. | |
dc.date.accessioned | 2021-04-05T03:22:35Z | - |
dc.date.available | 2021-04-05T03:22:35Z | - |
dc.date.issued | 2017 | |
dc.identifier.issn | 10139826 | |
dc.identifier.other | 2-s2.0-85027076469 | |
dc.identifier.uri | https://ir.swu.ac.th/jspui/handle/123456789/13174 | - |
dc.identifier.uri | https://www.scopus.com/inward/record.uri?eid=2-s2.0-85027076469&doi=10.4028%2fwww.scientific.net%2fKEM.737.595&partnerID=40&md5=d64250331290444f5a7f86bf5299d0bc | |
dc.description.abstract | The technique of stone-in-place casting has been established in jewelry production for three decades. However, the process is not widely used since it is limited to precious stones with high hardness and high stability at high temperature. This experiment tested tourmaline, which is a semi-precious gemstone having less hardness and less stability compared with precious stones. The objective was to achieve the conditions of a lost-wax casting process with tourmaline placed in waxes in the casting process. The experiment was divided into two parts. The first part was to understand the tolerance of tourmaline under the heating conditions. Natural tourmaline stones were investigated and compared inclusions tested at a temperature of 700°C. Tourmaline with ion-implantation was also heated to 700°C for comparison. The second part was to test tourmaline in-place casting with tree conditions of flask casting at 550°C, 625°C, and 700°C. The results showed that stones were able to tolerate as much as at 700°C. The inclusion growth of ion-implantation under heating to 700°C also observed the growth of inclusion in the same way as untreated tourmaline. The casting condition at 550°C showed better results. The highest probability of stones breaking after casting occurred in bezel settings. © 2017 Trans Tech Publications, Switzerland. | |
dc.subject | Casting | |
dc.subject | Gems | |
dc.subject | Hardness | |
dc.subject | Ion implantation | |
dc.subject | Ions | |
dc.subject | Casting conditions | |
dc.subject | Casting process | |
dc.subject | Heating conditions | |
dc.subject | High hardness | |
dc.subject | High temperature | |
dc.subject | Inclusion growth | |
dc.subject | Tourmaline | |
dc.subject | Tree conditions | |
dc.subject | Silicate minerals | |
dc.title | Lost wax casting conditions with tourmaline in situ | |
dc.type | Conference Paper | |
dc.rights.holder | Scopus | |
dc.identifier.bibliograpycitation | Key Engineering Materials. Vol 737 KEM, (2017), p.595-598 | |
dc.identifier.doi | 10.4028/www.scientific.net/KEM.737.595 | |
Appears in Collections: | Scopus 1983-2021 |
Files in This Item:
There are no files associated with this item.
Items in SWU repository are protected by copyright, with all rights reserved, unless otherwise indicated.